Abstract:
Forging forming of 6061-VIn aluminum alloy for automobile was forged by using different initial forging temperatures, final forging temperatures and forging speeds. The wear properties were tested and analyzed. The results show that with the increase of initial forging temperature, final forging temperature and forging speed, the wear volume of the aluminum alloy decreases first and then increases, and the wear resistance increases first and then decreases. At the initial forging temperature of 480 ℃, the final forging temperature of 360 ℃ and the forging speed of 15 mm/s, the wear volume of the sample is the smallest, and the wear performance is the best. The forging process parameters of the optimized 6061-VIn aluminum alloy sample are initial forging temperature of 480℃, final forging temperature of 360 ℃ and forging speed of 15mm/s.