Abstract:
W-9.5Ni
3Al-0.5YF
3 alloy was prepared by ball milling and spark plasma sintering (SPS). The effects of sintering temperature on the densification,phases,microstructure and mechanical properties of the alloy were analyzed. The results show that the distribution of YF
3 in the bonded phase is beneficial to reduce the densification sintering temperature of the alloy. The in-situ generated Al
2O